| Abrasion parameter of
keypad printing |
|

|
| |
Silk screen
printing, all color except Black |
Silk screen
printing, Black |
Silk screen
clear coating |
Sprayed
silicone clear coating |
Duracoat |
Encap |
Parylene |
| |
|
|
|
|
|
|
|
| Abrasion
resistance |
Poor |
Fair |
Good |
Good |
Excellent |
Superior |
Excellent |
|
Poor - under 10 cycles
Fair - 10 ~ 15 cycles
Good - 15 ~ 30 cycles
Excellent - 50 ~ 100 cycles
Superior - 100 ~ 200 cycles
|
|
Definition of failure:
Failure occurs when a printed line breaks or a second layer of color is exposed.
Abrasion test equipment:
RCA Abrasion Wear Tester:Norman Tool model #7 IBB.
Abrasion paper:Norman Tool paper type #1189
1 cycle of abrasion test equals about 10,000 times of finger press. |
|
|
|
Note :
|
The above is random figures for reference
only and is subject to change because of different
|
|
font style of different font style of the
graphics and key design. |
|
***Joesmen reserves the right to update any
information in this data sheet without any prior notice.*** |
|
|
|
|
|
abrasion|backlite|duracoat|design|encap|force-stroke curve|plas|printing|scs parylene coating|special rubber part|terminology
www.joesmen.com.tw
P.O.Box 36-357,Taipei,Taiwan 105,R.O.C﹒
5F-1,No.247,Sec.3 Pa-Teh Road,Taipei,Taiwan l05,R.O.C
Tel:886-2-25794501~3(3 lines)
Fax:886-2-25794601
E-Mail: joesmen@joesmen.com.tw
|